Ok. I guess that worked. Seems theres a max of two pics per post. Here is the general arrangement with my homemeade CC power supply with timers, amp meter and voltmeter on the right. All made from junkbox parts. Also a picture of the plastic drapes I can pull down to eliminate the fumes if any and direct them better into the range hood which is mounted above.