I always hesitate to "dedicate" anything. I'm forever changing my mind, but those are good suggestions. The screwdriver just happens to have a pretty straight nose on it and it is a easy press fit into the bracket I made so it is easily removed to become a screwdriver again. Although I never use it as such.
As for the welds - actually they were pretty bad looking so I ground and polished them flat. I haven't quite got the nice TIG "stack of coins" look down yet but I'm working at it.