Thanks for your reply. You might be on to something. After I apply the greaseless to the wheel I only waited about 30 seconds. When I stop the wheel, I see that the wheel is covered with compound and red all over the face. It certainly feels dry to the touch, but maybe its not. I thought I read from the manufacturer that it can be used immediately