View Single Post
  #2 (permalink)  
Old 06-09-2006, 12:09 AM
cruizer's Avatar
cruizer cruizer is offline
Amateur Metal Finisher
 
Join Date: May 2005
Location: Valpo, IN
Posts: 152
cruizer
Default Re: My flamed exhaust.

Third, cook to perfection.



Since they don't make high temperature vinyl that is easily removable after baking, I have make my own. I took high temperature tape (2" width) and layered it onto wax paper.
Reply With Quote