Default Re: Sodium Hydroxide (Caustic soda) Alternative

Quote:
Originally Posted by acidrain
Once the parts are stripped, immediately pull them and rinse. Go straight to the de-smut step.

How do you de-smut exactly?, are we talking chemically or by toothbrush!.