Default clear anodized 5052-T6 lightweight aluminum

How do I get this coating off of my grill so I can polish it? I just ordered the aluminum polishing kit, and the buffing kit that comes with 6 compounds. Is there something else I will need?

thanks,

djmas

these are the items I ordered

1/4 - 1/3 HP Buffing Kit
Hole Size: 1/2"

Aluminum & Copper Alloy Polishing Kit
Reply With Quote