View Single Post
  #7 (permalink)  
Old 04-26-2003, 01:06 AM
tperazzo tperazzo is offline
Newbie
 
Join Date: Jan 2003
Posts: 7
tperazzo
Default

What a difference 20 minutes makes. My problem was not letting the greasless compound dry on the wheel. Thanks guys!