Default Re: Black Oxide for Stainless

Per their online support, it shouldn't hurt the nylon in nyloc nuts. Craig didn't know about the weeping, but suggested using Seal45. This appears to be a coating ideally used on porous items, and leaves a smooth coat. It probably wouldn't hold up to having a wrench tightening it, maybe a few times. I think I get blackener and play with it.