Default Re: accuracy of the 720 rule

In regards to your question whether +-7% projected thickness is accurate enough I would hazard to guess that the answer for that question would lie with the customer. I would think that a customer who supplies an engineering drawing for their part would have a noted tolerance on the drawing. In my books, +-7% would be just fine!

Just my $0.02