You guys are gonna laugh at me when you see this oven LOL. It's acctualy an electrical cabinet. (I'm an electrician by trade) It's 3'x4'x16" with 7500W of heat. Now that I have visited this site and seen some of the ovens others are building, I am ashamed of mine LOL I wil eventually be building a 5'x6'x6' I think. Before winter. I only have a 18'x15' shop to work out of and I have a CNC mini MIll in there too. Kinda tight for space. Get's pretty hot in there when curing as well.