Default Is there something I can substitute for Nitric Acid?

I'm having adhesion troubles with plating aluminum & read that Zincate followed by Nitric Acid & a second dip in Zincate would solve this......problem is I can't find Nitric Acid anywhere locally.


Any Suggestions?