Default Re: Durability Question????

would want to say Nickel plating, because it's an electrosis process. But, it all depends on the application. Powder has more electrical resistance, like if it was valve covers and the power wire fromthe alt touches it, nickel will spark, powder will not.
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"