Quote:
Originally Posted by Banditperformance
I do know that you do not want to use glass bead on cast alum. Like intakes for example. The glass beads breakup and get imbedded in the alum and no amount of outgassing wil free them, untill you have powder sprayed on, then they will come up into the powder Ask me how I know lol
I have never heard that before, but I appreciate the warning!!! Tell us the whole story Bandit.
Mike