Re: Can you figure out what I did wrong?
Quote:
|
Originally Posted by callmej75
I did the same thing over an intake pipe a while back. I sandblasted, prepped with iron phosphate, outgassed at 8 minutes, shot the chrome, baked at 400* for 10 minutes, shot the liquid smoke at around 180*, cured at 400* for 20 minutes. Came out flawless.
|
Callmej75>what temp do you outgas at?
Johnny