Thread: Blast media???
View Single Post
  #3 (permalink)  
Old 06-19-2006, 10:14 AM
Livinincolor's Avatar
Livinincolor Livinincolor is offline
Amateur Metal Finisher
 
Join Date: Apr 2006
Location: Humble, Texas
Posts: 140
Livinincolor is on a distinguished road
Send a message via Yahoo to Livinincolor
Default Re: Blast media???

We are going to have to do the same thing or build a cabinet. Bags of blast media are getting a bit expensive!
We have tried a BUNCH of different types of media and the best we have used so far is BlastSand from White Caps (a subsidiary of Home Depot).
I am drawing up plans now for a custom cabinet so we can recycle the media. Letting it go into the lot along side the shop is a waste!
Johnny
__________________
Mike & Johnny
Sho Me Coatings
Reply With Quote