I use a product made by Mar-Hyde called tal strip. It is in the class of aircraft stripper and works very well on powder. I got it at my local automotive paint supplier. The key to this stuff is patience. I stripped some auminum wheels after useing chrome powder and clear on them and it took about half an hour to lift the powders from the wheel. Hope this helps!
Half an hour?
That would save me SOOO much time!