Re: copy chrome vs triple chrome plating
My kit is 25 gal. as far as the look I don’t see a difference in the cobalt steel and the nickel I have to say that if the part is prepped properly you can achieve the same look as triple chrome I my self plate for a lot of car clubs in this area and when I go to the shows I see my work everywhere.
I would have to say that if you asked Caswells for the cobalt steel anode the would send it with any buy although it is a little more expensive
__________________
Jim Eaton
|