Ok did a lil more research and correct me if I am wrong but the neutral will go to a1 on the contactor, the out #8 screw on the temperature controller will go to a2. Now from the schematics that stan sent I have to bridge #7 to #11 on the controller and run #11 and #12 to L1 and L2 correct

heopfully that is and wil just leave me with the wiring of the elements tkz again guys and hope this helps someone else out if they where totally lost like me