Well my first attempt at doing a fade with graphics...I did 1/3 in yellow(left it in too long) turned it around and did 2/3 in orange then bleached 1/3 off the orange end then did the red.Didnt quite fade(need more practice) Put on the decal and bleached the whole thing, then did the whole part black.Peeled decal(what a pain that was) scrubbed the residue with laquer thinner (another pain....stuff sticks good...10 year vinyl) Then sealed for 20.Good thing is i can strip it in 4 mins and redo it if wanted.
Thanks for all the tips and suggestions!!!
Ill try to get pics on tonight.