Ok did some quick test runs today and it take about 40-45 min. to reach 400 so I am thinking I might add 2 more elements since I have a more room to play with the 60 amp contactor, but let me ask when you cure do you start timing when you put item in and turn on the oven or when it reaches its tempeture then start clock?