Default Re: polishing ss knife blades

Quote:
Originally Posted by jimmijet2841
thanks for the imput i have finished the blades by sanding them starting with 400,600,1000 and finished them in 1200. that where i'm starting the polishing process from. i'm not sure if that changes anything. if it does please let me know. and once again thanks for taking the time to answer my questions.

jim
yes that changes the process greatly. since greaseless grit is close to equal grit of paper, then the 320 and 400 would be a great step backwards. i would start out with the felt bobs and green bar. if this does not give the lustre you want then back up a step to the brown bar or the black bar. then go foward again. as for the help, it is my pleasure bro.