Default Re: Black Oxide Process

Jim. I've heard that a predip in Caswell pre black solution followed by a standard Manganese Parkerizing treatment yields a very dark, rust resistant and durable finish. I have done both Zinc and Manganese Parkerizing before but have not used the pre-black solution. I am hoping that the color matches the AK black oxide finish more closely.

It might be worth a try.