I have priced it... and purchased some, I have a lot of Ti wire myself , I need to move half or more of it, forget the exact stuff I have tho LOL. I also noted when I used the wire (anodized with it) it turned a very dark color, black/purple, and swore it took die lol, I guess the dye just clung to the wire, because it washed off. The Ti is nice when you have alot of the same parts, not trie dthe screws yet, justa good snug threading that bottoms out will work good ?