I have been building a new oven 2x3x6. I have used metal studs with 22. gauge steel sheets to cover it. but I might have made a mistake using R20 Insulation (6") is this Insulation to big to fit in-between the oven walls? should I drill all the rivets off and re-insulation with the proper size? Please help i would like to start coating soon