Thread: Volts?
View Single Post
  #4 (permalink)  
Old 07-16-2006, 02:26 PM
nil8u nil8u is offline
Newbie
 
Join Date: Feb 2005
Posts: 18
nil8u
Question Re: Volts?

The video says to use .5A per pipe. Being as it has A surface area of 8sq".
So that would mean 2a for four pipes right? The solution says 1a per 16sq".
I am not getting any plate at all so I dont think the amps are too high. Too low if anything.
What manual do you have? Mine sucks it doesnt have $#it. So many questions un answered like how many times can I use a hanger wire.
Reply With Quote