Re: Volts?
Thanks Fly I appreciate your help. The copper single pipe is coming out looking just as it went in. No plating whatsoever. I think I might have A problem with the electrical connections. I'm going to rewire and try again. One more question... is the nickel activated when it comes out of the nickel tank? Do I have to pickle before I go into the chrome or can I rinse and go straight into the chrome? Thanks again fly!, Lance
|