View Single Post
  #4 (permalink)  
Old 07-18-2006, 08:06 AM
griffsfsr griffsfsr is offline
Newbie
 
Join Date: Feb 2004
Posts: 5
griffsfsr
Default Re: First parts and some questions

Thank you for the comments and suggestions. I have heard good things about zoop seal although this is the first time I have heard about Glare. In my internet travels I came across a Clear POR 15. Has any one heard of it and tryed it? I looked at the part last night and it had started to surface rust. I was surprised to see this since it had sat in my car for almost three weeks with no rust. I worked on sanding the part more a couple of days ago, even those areas had some rust. I think it might possibly be from touching it. It has been really hot here lately and I was sweating a bunch. Thank you again for the comments.