Hello, I have a copy chrome kit that I havent used in two years. When I opened the container with the solution it was still green however there was a 1/4" or so of a caked residue on the bottom of the container. Is this normal? should I reagitate it back into the solution or is this some sort of contaminate from previous plating projects? Thanks for your input