Re: My first Ano - Am I color blind?
ok i guess you could call that chalky. So that is was dissolution looks like.
0.5 mill and 8-per sqr foot was what i was going for on that run.
from hear on out I am gona go 5.5 amps per sqr feet due to the limits of my supply and the runs i intend to do with this tank.
As far as temp goes i don't think it was an issue. standing water in that room was about 60F and i wasn't pumping all that much wattage into it. I could drop one of those HDPE ice gel pac things in there to make it nice and cool
as far as acid concentration goes i see 1:3 as being the golden number. that was what I was going for but i seemed to have messed it up.
how dose 64 flOZ of bat acid and 1.5 gals of water sound?
water did not beed on the prepped surface so I am fine there.
Now i hope someone can answer this one. Dose caswells A4 Yellow Look orange when mixed with water. I am really worried now that they shipped me the wrong dye.
|