My suggestion would be to add the d/s water that has evaporated heat the solution up to approx 170 or better while cooling be sure to stir the solution to help dissolve the crystals . Let the solution sit for 24 hours to cool then heat to 75 to 110 and plate a dummy item to check for brightness add brightener as needed