Preparation question
Hi, I just ordered a copy chrome plug and plate kit and have some questions about preparation. Here's the steps I plan to use for mostly bolts, washers and large nuts.
1. Clean/Sand and Buff Part.
2. degrease w/comet mixed with warm water. (1/2 hour soak)
3. Remove rust in muriatic acid/water.
4. dip in degreaser solution.
4. Spray part with distilled water.
5. Plug N plate.
Does this sound right? After I spray part with distilled water, should I let it dry then plate? Or can I plate right away after the distilled water spray? Thanks and wish me luck.