Default Re: Definition of preparation

when quoting a price i give a price for the total job. if questioned about it i then detail all the prep and steps needed. as was told to me by a friend, when you tell them the price and the dont run away, but look like they just passed a kidney stone you are in the right range. this should not be a "cheap" alternative to paint for the customer, since in most cases it is a better finish than liquid finish anyway.
__________________
when in doubt polish it out/ why replace it when you can refinish it