Ok, I got my pound each of Xtreme and Super Clear in the mail today and am ready to shoot some parts. However, when I read the write-up by Hvac36, it says "Now Cure at 375 for 30 mins,", but the can of Xtreme says 392 for 30 min. If I bake at 375, will it cure or is this reduced temp part of the "Magic" to prevent the clouding and greying?
Just read the can of clear and it also says 392 for 30. So.... heat the Xtreme back to 150, coat, and then to "the required time" for clear? 392 or 375? Doh!!! (scratching head)
BTW thanks for the write-up Hvac36, I'm sure it has helped many get the results they wanted! I, on the other hand, am easily confused and slow!!!
Later