Re: Pre Heating
I only leave the vinyl on until flow out. I recently coated a pair of Yahama wheels and I masked 4 times before I finally used the vinyl and all the other tapes lifted terribly and the vinyl was easy to form into the curves of the wheels with no lifting as all.
Jason
|