Yes - you need to use a <a href="/alzinc.htm" target="_blank">Non-Acidic nickel bath</a>, otherwise the acidic nickel will corrode the cadmium.

Sure, you can spot plate with a brush plating system.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote