The trim I am polishing is from a 1954 car so it is reasonably thick and not too subject to warpage. I thought heat was my friend in polishing so if the piece warmed up a little so much the better. Also, it is a soft cotton wheel so the pressure on the wheel will be minimal. Thanks for the previous post but I guess I'm just amazed that 3400 rpm spindle speed and a 10 inch wheel are too much.
|