Just some additional suggestions to what mpierich stated. Try using a die grinder with cartridge rolls. You can get just about any grit, and diameter, you will need in cartridge rolls. It looks like you have a lot of round area to do which may make it easier. You can also load 1" and larger diameter buff with greaseless and go at it that way. I have used a 3/8" drill motor with up to a 4" buff on it for greaseless and it works fine.
John
|