Default

I think it was the bath temp.

I am sure it is 6061, I buy my bar from a reputable dealer, and it is labeled very well.

I have done blasted parts before, with good results, just not red.

I re-did the "pink" frame today, and the bath temp was a bit lower. (Cooler outside)

It held its color better, but I also used a different dye.

I used to steam my parts, but that led to streaking, the boiling gives me a much more consistent color.

Thanks for all your help guys, I really appreciate it.