Same 3/4 in 1/2 out.

Right now I am using the pump for the chiller.I think its a little much, I had to restrict the flow so the water could chill. I will pick up a much smaller pump Monday for that.

I do have 1/2 CPVC run in the tank with about 20 1/16 holes that seems to agitate pretty well with a transfer pump I have. It is about 300 GPH but got tired of listening to it.