Hmmm... it's most definately is 5xxx alloy (as marked on your package).
That only leaves the ano process. There must be some variable between this run, and your successful previous runs. I have to think that the thinner wire may be heating up.
Is it possible that the coil of thinner wire is creating a resistor? Maybe a test run of un-coiled wire.
Sorry, it's the only thing I can think of right now.