Thread: Copy Chrome?
View Single Post
  #2 (permalink)  
Old 09-11-2006, 03:54 PM
jimcarry's Avatar
jimcarry jimcarry is offline
Experienced Metal Finisher
 
Join Date: Jul 2004
Location: Arkansas
Posts: 370
jimcarry is on a distinguished road
Send a message via Yahoo to jimcarry
Default Re: Copy Chrome?

There are a few main reasons I chose copy chrome
one is for the safety the product dose not let off harm full fumes like regular chrome
the other reason is it is not EPA regulated it is a cobalt solution and with the larger kits you will use a cobalt steel anode and thus far I have not had any durability problems at all it has all the appearance of chrome with out the EPA problems
__________________
Jim Eaton
Reply With Quote