Default Re: want educated on caswells new gun

Yes, It works 10 times better than a hobby gun, as far a charging the powder. It still has it's limits though, being based on a hobby gun. I've learned over the years to adjust for the inconsistent flow of powder from the hobby gun. Even with a "custom" nordson 100, I'll grab my hobby gun first as I can change colors 20 times in a normal day.

I'm working on a small hopper for the new hobby gun, if it works like I hope there will be a nordson for sale(Well that may be pushing it!!)