Angry Stickey triger

Anyone having a problem with the (Caswell hobby gun) triger sticking and not being able to turn off the powder stream? I have taken the triger mechinism apart and cleaned it very well, and it works smoothly until I apply powder and it starts sticking again. This unit is about a month old and I have had this problem since day one.