Default Black anodize dye doesn't take

I black anodized a part.

The part was cleaned, anodized in battery acid and then dipped in distilled water with a few drops of Caswell black dye. Everything went well.

I have tried the same process several times again with different parts. No matter what I do he parts do not take the dye.

I do not understand why the process doesn't work.

Can anyione suggest what I'm doing wrong?