I plated a part that was flash copper'ed first. Copper was flawless, looked excellent. Didnt polish copper, just rinsed and went to CC. Plated part for 30 minutes, and it looked fine in some places (mostly the rear of part) and all over the face it had pits. ( possibly bubbles? ) I had aggitation going strong, but it may have been missing the front of part, I dunno. Anyway, this is a $100 part that takes 6 hours to machine...anyway to remove plating with destroying part? Or should I just trash it now. I would love to leave the copper, but at this point I dont care.