I have been getting better at PCing parts and have been getting good finishes, mostly. I have noticed that the Super Wet Black coated parts are easily scuffed. If there is any dust on the part and I brush it off with my finger, the surface will have light scratches or scuffs on it. Are the parts not fully cured (either under or over cured) or is that the nature of the Super Wet Black?