Default Re: Sanding the hard spots.

Quote:
Originally Posted by jrow
68commando, chcustom

Third they make cartridge rolls in 1/4" diameter in different grits that will work real well. You will have to get a different mandrel to use these because of their diameter. And along with what sswee states the Cratex will work also.

John
The ones I get use the same mandrel as the larger ones.