Default anodizing/blasting

the parts are aluminum there blasted then sent to be anodized,after anodizing there is dirty looking areas on the parts,not always the same spot , part ,or even the same color,sometime its a dark looking dirt and sometimes its a white haze.any ideas on what it is or how to try to stop it from forming on the parts?is it something in the blasting the anodizing or what