I redid the rest an vualla. a bright and shinny piece came from the depths of electrolite and it does match the bow..
I did over amp the part and kept it in to long.I'm still learning ,and have a long way to go,but I think its worth travelling.My next baby steps will start with PH,tank cooling and many other things ,but I'll be there soon enough.
If anyone has any suggestions PM me I'm all ears..
Thanks again Acidrain for all your help..
|