This is a case of the customer never being right. He simply can't 'choose' his anodize color. The chemistry involved in anodize colors will only allow a limited range of colors. It isn't like paint. eg: you can't do white!
Better that you tell him what you CAN do, and he chooses on one of those.
Now, if you can perfect mixing several existing colors, and provide a consistant result, all credit to you. Make sure you charge him accordingly.
|